上海尚南新材料有限公司

ST 2000

ST 2000 starch ether can obviously improve the consistence and enhance the yield stress of fresh mortar, thus greatly preventing the slipping  of tiles. Good synergy effect can be achieved if Ashland cellulose ether is used together.

ST 2000 can be applied in neutral and alkaline mortar systems. It is widely compatible with additives such as cellulose ether, redispersible polymer powder, air-entraining agent, which is conducive to enhance the adhesion of mortar system.


Properties 


Appearance

White or yellow powder

Moisture content

<10 %

Particle size

Max.3 % > 0.8 - 1 mm

Viscosity

300 - 800 mPa·s

Remarks: Testing conditions for viscosity——2 % water solution, Brookfield RV viscometer, 20 ℃,100 rpm

 

Applications 


It is recommended to be applied in mortar system with medium to high viscosity,including but not limited to:

 > Borad insulation system 

 > Slurry insulation system 

 > Cement / gypsum based stone adhesive